We Minimise Manuel Welding Defects in a Mechanised Manner

With our submerged arc welding machine, we minimise manuel welding defects in a mechanised manner, which corresponds over 30% improvements in labour and process completion durations. All welds applied by our submerged arc welding machine have been successfully passed NDT examinations and continuously assure Selnikel quality.